Microstructures and high-temperature failure analyses of 25Cr-35Ni-Nb + MA/32Cr-20Ni-Nb dissimilar welded joint with different filler wires
  • Affiliation of Author(s):
    材料科学与工程学院
  • Journal:
    Materials and design
  • Key Words:
    Filler wire;Fracture;High-temperature performance;HP steel;Microstructure;Precipitate