WANG Weiqiang
Professor
Visit:
Personal Information:
  • Name (English):
    WANG Weiqiang
  • Name (Pinyin):
    Wang Weiqiang
  • Date of Employment:
    1976-09-01
  • School/Department:
    School of Mechanical Engineering
  • Administrative Position:
    Professor
  • Education Level:
    Postgraduate (Doctoral)
  • Business Address:
    Room 802, Innovation Building
  • Gender:
    Male
  • Contact Information:
    Mobile Phone:+86 13325116881
  • Degree:
    Doctoral Degree in Engineering
  • Status:
    Employed
  • Alma Mater:
    East China University of Science and Technology
  • Supervisor of Doctorate Candidates
  • Supervisor of Master's Candidates
Discipline:
Chemical Process Equipment;
Materialogy;
Chemical Engineering;
Mechanical Engineering;
Education
  • 1978-2 — 1982-1
    Shandong University of Chemical Technology
    Chemical Process Equipment
    Bachelor's Degree in Engineering
  • 1982-2 — 1984-9
    East China University of Chemical Technology
    Chemical Process Equipment
    Master's Degree in Engineering
  • 1986-9 — 1990-3
    East China University of Chemical Technology
    Chemical Process Equipment
    Doctoral Degree in Engineering
Publication
Papers

1. 陈宇鑫. 响应面法优化CO_(2)亚临界态萃取等压超临界态分离核桃油工艺 .粮食与油脂.2023,36 (3):53-55

2. 陈宇鑫. 响应面法优化CO2亚临界态萃取等压超临界态分离核桃油工艺 .粮食与油脂.2023,36 (03):53-55+71

3. 侯凯文. 基于均匀设计的花生油亚/超临界CO2等压连续萃取分离工艺研究 .中国粮油学报 ?.2023 :1-7

4. 李建勋. Mechanism and Method of Testing Fracture Toughness and Impact Absorbed Energy of Ductile Metals by Spherical Indentation Tests .Chinese Journal of Mechanical Engineering (English Edition).2023,36 (1)

5. 刘国祎. 响应面法和人工神经网络对亚临界CO2萃取红花籽油的建模与优化 .《食品工业科技》.2023 :1-13

6. Wang, Pengfei. Effects of Specimen Size and Welded Joints on the Very High Cycle Fatigue Properties of Compressor Blade Steel KMN-I .COATINGS.2021,11 (10)

7. Wang, Pengfei. Research on Residual Life Estimation Method for KMN Steel Based on Nonlinear Ultrasonic Testing .Applied Sciences-Basel.2021,11 (23)

8. 陈明亚. Safety assessment of the small welded pipe system by the test and FEA .INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING.2021,194

9. Wang, Pengfei. Fatigue Damage Evaluation of Compressor Blade Based on Nonlinear Ultrasonic Nondestructive Testing .Journal of Marine Science and Engineering.2021,9 (12)

10. 王鹏飞. Effects of microstructure and inclusions on very high cycle fatigue properties of compressor blade steels .Strength Fract. Complex..2017,10 (1):1

11. 张泰瑞. A STUDY ON THE BALL INDENTATION TEST FOR LINEAR HARDENING METALS .PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2017, VOL 7.2017

12. Zhang, Zhuo. Experimental Study on the Throttling Effect of SC-CO2 Containing Ethanol System Flowing Through the Coaxial Annular Nozzle and the Prediction Based on Artificial Neural Network .INTERNATIONAL JOURNAL OF THERMOPHYSICS.2021,42 (11)

13. Zhang, Zhuo. Experimental Study on the Throttling Effect of SC-CO2 Containing Ethanol System Flowing Through the Coaxial Annular Nozzle and the Prediction Based on Artificial Neural Network .INTERNATIONAL JOURNAL OF THERMOPHYSICS.2021,42 (11)

14. 张泰瑞. Improving the tensile property calculations with plastic zone radius measurements in depth-sensing spherical indentation tests .JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN.2021

15. Zhang, Zhuo. Establishment of the Predicting Models of the Dyeing Effect in Supercritical Carbon Dioxide Based on the Generalized Regression Neural Network and Back Propagation Neural Network .PROCESSES.2020,8 (12)

16. 张泰瑞. A strain-pattern-based spherical indentation method for simultaneous uniaxial tensile residual stress and flow property determination .JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN.2021,56 (1):50

17. 张泰瑞. An energy-based method for flow property determination from a single-cycle spherical indentation test (SIT) .INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES Journal.2020,171

18. WANG Weiqiang , liaiju  and 张泰瑞. THE SPHERICAL INDENTATION APPROACH FOR FRACTURE TOUGHNESS EVALUATION: A STUDY BASED ON THE ENERGY RELEASE RATE .2018

19. WANG Weiqiang. Structural Integrity Analysis of Two Over-Temperature Methanation Furnaces .Journal of Failure Analysis and Prevention.2019,19 (1):230

20. WANG Weiqiang. A comparative study on uniaxial tensile property calculation models in spherical indentation tests (SITs) .International Journal of Mechanical Sciences.2019,155 :159

21. WANG Weiqiang. A study on determination of tensile properties of metals at elevated temperatures from spherical indentation tests .JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN.2019,54 (5-6):331

22. WANG Weiqiang. A comparative study on fracture toughness calculation models in spherical indentation tests (SITs) for ductile metals .International Journal of Mechanical Sciences.2019,160 :114

23. WANG Weiqiang. Dynamic Stress Analysis of Multilayered Structure with Radial Gaps of Cylindrical Pressure Vessel under Plane Strain Conditions .Journal of Pressure Vessel Technology, Transactions of the ASME.2019,141 (4):41202

24. WANG Weiqiang. Three-dimensional finite element analyses of repair process and safety margin assessment .International Journal of Pressure Vessels and Piping.2019,172 :283

25. WANG Weiqiang  and 张泰瑞. Determination of the proof strength and flow properties of materials from spherical indentation tests: An analytical approach based on the expanding cavity model .Journal of Strain Analysis for Engineering Design.2018,48 (4):225

26. WANG Weiqiang  and 张泰瑞. A constitutive model independent analytical method in determining the tensile properties from incremental spherical indentation tests (ISITs) .International Journal of Mechanical Sciences.2018,34 :2019

27. WANG Weiqiang  and 张泰瑞. Improved methods to determine the elastic modulus and area reduction rate in spherical indentation tests .Materialpruefung/Materials Testing.2018,32 (4):355

28. WANG Weiqiang , lijianfeng  and 王鹏飞. Research on fatigue damage of compressor blade steel KMN-I using nonlinear ultrasonic testing .Shock and Vibration.2017,22

29. WANG Weiqiang. Urea reactor integrity evaluation based on failure analysis .Journal of Pressure Vessel Technology, Transa.2007,v 129 (n 4):744

30. WANG Weiqiang. Application of the Analytic Hierarchy Process in Risk Analysis for Urea Reactor .2nd International Conference on Risk Manageme.2008

31. yumeijie , WANG Weiqiang  and wangchengguo. Thermal Properties of Acrylonitrile/Itaconic Acid Polymers in Oxidative and Nonoxidative Atmospheres .Journal of applied polymer science.2010,116 (2):1207

32. WANG Weiqiang , Yanpeng Qu  and liaiju. 超臨界流體噴染及其流場數值模擬研究 .第十一届2012年超临界流体技术应用与发展研讨会暨第二届海峡两岸超临界流体技术研讨会.2012

33. WANG Weiqiang  and Yanpeng Qu. 超临界流体多过程试验平台研究 .第十届全国超临界流体技术学术及应用研讨会论文集.2014

34. Yanpeng Qu  and WANG Weiqiang. Novel Multi-Stream Plate Exchanger under High Pressure—Structure and its Design Method .Advanced Materials research.2014,1062 :658

35. WANG Weiqiang. 尿素合成塔液相泄漏蒸气爆炸压力计算 .化肥工业.2012,39 (2)

36. WANG Weiqiang. 尿素合成塔爆破原因分析综述 .机械强度.2012,34 (3):427

37. Yanpeng Qu  and WANG Weiqiang. 用于超临界流体工艺过程的板式换热器 .第九届全国超临界流体技术学术及应用研讨会文集.2012

38. Yanpeng Qu  and WANG Weiqiang. 超临界流体技术制备超微粉体用径向组合型喷嘴 .2008第七届全国超临界流体技术学术及应用研讨会.2010

39. WANG Weiqiang. FAULT TREE ANALYSIS ON SEAL FAILURE OF HIGH PRESSURE AMMONIUM CARBAMATE PUMP .Proceedings of the 3rd World Congress on Engi.2008

40. Yanpeng Qu , WANG Weiqiang  and liaiju. SCF快速膨胀过程流动模拟及其工艺参数的影响 .2008第七届全国超临界流体技术学术及应用研讨会.2008

41. WANG Weiqiang. 基于ANSYS Workbench和FLUENT的超临界二氧化碳萃取釜流场模拟及其结构改进 .《化工进展》.2012,31 (9):1914

42. Yanpeng Qu , WANG Weiqiang  and liaiju. 喷嘴和结晶器结构及参数对SAS法制备超微粉体的影响 .第八屆2009年超臨界流體技術應用與發展研討會.2009

43. WANG Weiqiang. 奥氏体不锈钢换热管应力腐蚀开裂分析 .《化工机械》.2012

44. WANG Weiqiang , liaiju  and Yanpeng Qu. 超临界流体多工艺过程试验平台的模块化设计 .第九届全国超临界流体技术学术及应用研讨会文集.2012

45. WANG Weiqiang  and Yanpeng Qu. 超临界流体技术制备超微粉体喷嘴结构设计 .中国粉体工业.2007

46. WANG Weiqiang. 局部冲击压力下多层包扎容器弹性动力响应分析 .石油化工设备.2012,41 (3):34

47. WANG Weiqiang. 活塞式压缩机联轴器连接螺栓断裂原因分析 .理化检验-物理分册.2012,48 (3):203

48. WANG Weiqiang. 超临界流体技术制备超微粉体的新型喷嘴 .《化工机械》.2008,35 (6):374

49. WANG Weiqiang. 尿素合成塔爆炸载荷类型与破坏形态的关系分析 .山东大学学报(工学版).2008,38 (3):51

50. WANG Weiqiang. 磁致伸缩导波技术检测管道缺陷 .《无损检测》.2008,30 (7):434

51. WANG Weiqiang. 多层包扎尿素合成塔应力状况分析 .机械强度.2008,30 (1):93

52. WANG Weiqiang. WNN优化模型在模拟超临界二氧化碳中固体溶解度的应用 .天然气化工(C1化学与化工).2008,33 (3):75

53. WANG Weiqiang. 平阴尿塔的物料和爆炸能量估算 .山东大学学报(工学版).2008,38 (3):46

54. WANG Weiqiang  and Yanpeng Qu. 新型超临界流体染色器设计 .2008第七届全国超临界流体技术学术及应用研讨会论文集.2008

55. WANG Weiqiang. Urea reactor integrity evaluation based on failure analysis .Journal of Pressure Vessel Technology, Transa.2007,v 129 (n 4):744

56. WANG Weiqiang. 氨合成废热锅炉换热管应力腐蚀开裂分析 .《压力容器》.2008,25 (3):41

57. liaiju , WANG Weiqiang  and 李爱菊. 聚苯硫醚/石墨基双极板复合材料性能的研究 .《人工晶体学报》.2008,37 (4):819

58. WANG Weiqiang. Structural and Regulating Characteristics of Adjustable Annulus-clearance Nozzle Used in Supercritical Fluid Precipitation .武汉理工大学学报(材料科学版)(英文版).2017,32 (6):1487

59. WANG Weiqiang , Yanpeng Qu  and liaiju. Structural and regulating characteristics of adjustable annulus-clearance nozzle used in supercritical fluid precipitation . Journal Wuhan University of Technology, Materials Science Edition.2017,32 (6):1487

60. WANG Weiqiang. 尿素合成塔层板严重腐蚀开裂分析 .化工机械新技术研究进展.2008

61. WANG Weiqiang. 磁致伸缩导波技术在构件腐蚀检测中的应用实践 .无损探伤.2008,2008年卷 (5):18

62. WANG Weiqiang. 水溶液全循环尿素生产装置中静设备失效类型和机理研究 .化工机械新技术研究进展.2008

63. WANG Weiqiang. 疲劳概率模型的综合评价方法 .中国机械工程.2008,19 (23):2812

64. WANG Weiqiang. 平阴尿塔塔体爆炸能量分析与计算 .山东大学学报(工学版).2008,38 (4):80

65. WANG Weiqiang. 合成氨装置风险预测控制系统的研究 .化工机械新技术研究进展.2008

66. WANG Weiqiang. 尿素合成塔物料蒸气爆炸初步研究 .化工机械新技术研究进展.2008

67. WANG Weiqiang. 锅炉汽包至上集箱间联络管爆破原因分析 .《压力容器》.2008,25 (10):33

68. WANG Weiqiang  and zhanglewen. FEM analyses of stress and deformation of a flexible inner pressure bolt .Journal of China University of Mining and Tec.2008,18 (4):584

69. WANG Weiqiang. Catastrophic Explosion of a Multilayered Urea Reactor .Ammonia Plant Safety and Related Facilities.2008

70. WANG Weiqiang. Application of the Analytic Hierarchy Process in Risk Analysis for Urea Reactor .2nd International Conference on Risk Manageme.2008

71. WANG Weiqiang. 尿素合成塔风险分析 .腐蚀科学与防护技术.2008,20 (5):377

72. WANG Weiqiang. 尿素合成塔层板开裂规律及原因分析 .全国化工过程机械博士研究生创新研讨会论文摘要集,2009,南京.2009

73. WANG Weiqiang. 锅炉水冷壁管腐蚀爆裂失效分析 .压力容器先进技术——第八届全国压力容器学术会议.2013

74. lijianfeng , WANG Weiqiang  and sunjie. Effect of cracked blade distribution on vibration characteristics of centrifugal impeller .Applied Mechanics and Materials.2013

75. WANG Weiqiang. Failure analysis of spiral plate heat exchanger .Applied Mechanics and Materials.2011

76. WANG Weiqiang  and liaiju. Study on the microstructure of 20 steel with strain aging .Proceedings of ASME 2011 Pressure Vessels and.2011

77. WANG Weiqiang. Failure analysis of 20G boiler tubes .International Symposium on Structural Integri.2010

78. WANG Weiqiang  and liaiju. 避免Q245钢厚壁高压管应变时效脆化的试验研究 .第七届全国压力容器学术会议论文集.2009

79. WANG Weiqiang. Root cause analysis of stress corrosion at tube-to-tubesheet joints of a waste heat boiler .Engineering Failure Analysis.2014,45 :398

80. WANG Weiqiang. 通过标准规避高压钢管应变时效脆化的发生 .《压力容器》.2010,27 (11):45

81. WANG Weiqiang  and Yanpeng Qu. 超临界流体喷染的原理及研究进展 .第十届全国超临界流体技术学术及应用研讨会论文集.2014

82. WANG Weiqiang. Research on the properties of 20G steel with strain aging embrittlement using indentation test .East China University of Science and Technology Press,2012.2012

83. WANG Weiqiang. The pressure variation of BLEVE triggered by liquid release through a crack in the cylindrical pressure vessel .East China University of Science and Technology Press,2012.2012

84. WANG Weiqiang , wangyanming  and liaiju. Effect of fiber surface treatment techniques on properties of short carbon fiber reinforced phenol formaldehyde resin/graphite composite bipolar plate .Advanced Materials research..2011

85. WANG Weiqiang. Preparation of ultra-fine powder using supercritical fluids: A review .Applied Mechanics and Materials.2011

86. WANG Weiqiang  and liaiju. 消除Q245钢应变时效脆化的理论分析及试验研究 .第七届全国压力容器学术会议论文集.2009

87. WANG Weiqiang. The stress corrosion cracking of austenitic stainless steel heat exchange tubes—three cases study .Proceedings of the ASME 2010 Pressure Vessels.2010

88. WANG Weiqiang  and liaiju. The Fracture Failure Analysis of a Hot Pure Water Storage Container .Procedia Engineering.2015

89. WANG Weiqiang  and Yanpeng Qu. Effects of austenitic stainless steel tube and tubesheet hole dimensional deviations on the hydraulic expansion pressure .International Journal of Pressure Vessels and Piping.2016,138 :1

90. WANG Weiqiang  and Yanpeng Qu. A Fortran implementation of isogeometric analysis for thin plate problems with the penalty method .Engineering Computations.2016,33 (7):2149

91. WANG Weiqiang. Using FEM to predict residual stresses in girth welding joint of layered cylindrical vessels .International Journal of Pressure Vessels and Piping.2014,119 :1

92. WANG Weiqiang  and lijianfeng. Fatigue behavior and mechanism of FV520B-I in ultrahigh cycle regime .Procedia Materials Science.2014

93. WANG Weiqiang. Residual stresses in the welding joint of the nozzle-to-head area of a layered high-pressure hydrogen storage tank .International journal of hydrogen energy.2014,39 (21):11061

94. WANG Weiqiang. On-Line monitoring method for centrifugal compressor and impeller remanufacturing .East China University of Science and Technology Press,2012.2012

95. WANG Weiqiang. Failure analysis of a bellows expansion joint of inconel625 alloy .Advanced Materials research.2012

96. WANG Weiqiang. 甲胺反应器严重开裂原因分析. .第七届全国压力容器学术会议论文集.2009

97. WANG Weiqiang  and liaiju. Study on the Brittle Fracture of the Q245 Steel High Pressure Piping in an Ammonia Synthesis Unit .The 12th International Conference on Pressure.2009

98. WANG Weiqiang  and liaiju. Analysis on layer cracking of urea reactors .Proceedings of the ASME 2010 Pressure Vessels.2010

99. WANG Weiqiang  and liaiju. The stress distribution and critical c rack length analysis of a cracked multilayer urea reactor .East China University of Science and Technology Press,2012.2012

100. WANG Weiqiang  and Yanpeng Qu. 重整氢压缩机连杆螺栓断裂失效分析 .金属热处理.2016,41 (2):200

101. WANG Weiqiang. 20(G)板不同焊接缺陷的磁记忆信号检测分析 .中国特种设备安全.2016,32 (5):33

102. WANG Weiqiang  and Yanpeng Qu. 基于场协同原理的管道经济管径计算新方法 .流体机械.2016,44 (8):32

103. WANG Weiqiang. A New Method to the Elastodynamic Response of a Spherical Shell Under the Impact Load .Journal of Pressure Vessel Technology.2016,138 (3):345011

104. WANG Weiqiang  and Yanpeng Qu. Probability Analysis of Pit Initiation on Austenitic Stainless Steels .Procedia Engineering.2015

105. WANG Weiqiang. The Measurement of Mechanical Properties of Pipe Steels in Service through Continuous Ball Indentation Test .Procedia Engineering.2015

106. WANG Weiqiang  and Yanpeng Qu. Failure analysis of austenitic stainless pipes in amine liquid regeneration unit of a desulfurizer .Engineering Failure Analysis.2015,57 :164

107. WANG Weiqiang. 水冷壁管开裂原因分析 .化工装备.2015 (2):37

108. WANG Weiqiang. 连续球压痕法测试压力容器钢力学性能的研究 .振动.测试与诊断.2015,35 (2):281

109. WANG Weiqiang. Failure analysis of stress corrosion cracking in heat exchanger tubes during start-up operation .Engineering Failure Analysis.2015,51 :1

110. WANG Weiqiang  and lijianfeng. Fatigue behavior and mechanism of FV520B in very high cycle regime .Strength, Fracture and Complexity.2015,9 (2):161

111. WANG Weiqiang. Mathematical model for tension of textile during the process of supercritical fluids spray dyeing .Advanced Materials Research.2014

112. WANG Weiqiang. 法兰密封系统应力松弛有限元分析 .《压力容器》.2013,30 (4):23

113. WANG Weiqiang. Study on the strength of textile during the process of supercritical fluids spray dyeing .Advanced Materials Research.2014

114. WANG Weiqiang. SCF preparation of drug particle using size adjustable nozzle .Key Engineering Materials.2012

115. WANG Weiqiang , Yanpeng Qu  and Songying CHEN. Significance analysis on influential factors of stress corrosion based on grey relational theory for stainless steels .East China University of Science and Technology Press,2012.2012

116. WANG Weiqiang. The feasibility of research for shell deformations with isogeometric analysis .East China University of Science and Technology Press,2012.2012

117. WANG Weiqiang. Failure analysis of the pure zirconium hanging sample for acetic anhydride reactor .East China University of Science and Technology Press,2012.2012

118. WANG Weiqiang. Numerical investigation on weld residual stresses in tube to tube sheet joint of a heat exchanger .International Journal of Pressure Vessels and Piping.2013,101 :37

119. lijianfeng , WANG Weiqiang  and sunjie. Effect of cracked blade distribution on strength of centrifugal impeller .Applied Mechanics and Materials.2013

120. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on developed solution structure theorem for wave equation .Journal of Pressure Vessel Technology, Transactions of the ASME.2011,134 (1):112101

121. WANG Weiqiang. Analysis on elastoplastic stress distribution in a layered cylindrical vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transactions of the ASME.2012,134 (3):312061

122. WANG Weiqiang. Solution of gas explosion load and simulation of dynamic response of multilayer structures .Advanced Materials research..2012

123. WANG Weiqiang  and Yanpeng Qu. Supercritical fluid pray dyeing: A new method of dyeing and simulations of its flow field. .Advanced Materials research.2011

124. WANG Weiqiang  and liaiju. 热处理避免和消除20钢厚壁高压管应变时效脆化实验研究 .《材料工程》.2011,2011年卷 (1):57

125. WANG Weiqiang , Yanpeng Qu  and guancongsheng. 管壳式固定床反应器爆炸事故分析 .《化工机械》.2010,37 (2):222

126. WANG Weiqiang. 我国特种设备事故调查与处理体制的思考 .中国特种设备安全.2010,2010年卷 (7):33

127. WANG Weiqiang  and liaiju. A simplification method of defects in multilayered vessels detected by acoustic emission detection .Fracture Mechanics and Structural Integrity S.2009

128. WANG Weiqiang. The exploration of strain aging embrittlement evaluation in metallic materials using indentation test .Proceedings of 2011 International Symposium o.2011

129. WANG Weiqiang  and liaiju. Study on the composites of phenol formaldehyde resin/graphite reinforced by milled carbon fibers for bipolar plates .Advanced Materials Research.2010

130. WANG Weiqiang. Grey predication of corrosion on oil atmospheric distillation equipment .2009 4th IEEE Conference on Industrial Electr.2009

131. WANG Weiqiang  and Yanpeng Qu. Preparation of Cefquinome Nanoparticles by Using the Supercritical Antisolvent Process .Journal of Nanomaterials.2015,2015(ID: 767945 ) :1

132. WANG Weiqiang  and liaiju. Failure analysis of the brittle fracture of thick-walled 20 steel pipe in an ammonia synthesis unit .Engineering Failure Analysis.2010,17 (6):1359

133. WANG Weiqiang. 我国高压管道标准中某些规定存在的问题与思考 .压力管道技术研究进展精选集——第四届全国管道技术学术会议,2010 .2010

134. WANG Weiqiang. Grey decision on oil distillation tower top exchangers maintenance overhaul .2009 4th IEEE Conference on Industrial Electr.2009

135. WANG Weiqiang  and lijianfeng. 连续球压痕测定常用叶轮材料力学性能的研究 .流体机械.2015,43 (2):7

136. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on generalized solution structure theorem for wave equation .Proceedings of the ASME 2010 Pressure Vessels.2010

137. WANG Weiqiang. Modified formulation of layer stresses due to Internal pressure of a layered vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transa.2010,132 (5):5120101

138. WANG Weiqiang. A Fortran implementation of isogeometric analysis with superiority in convergence and accuracy .Procedia Engineering.2015

139. WANG Weiqiang  and Yanpeng Qu. 超临界流体染纱器现状与新型结构 .《现代化工》.2010,30 (7):65

140. Lester , WANG Weiqiang , LI Fangyi  and lijianfeng. Damage mechanism and evaluation model of compressor impeller remanufacturing blanks: A review .Frontiers of Mechanical Engineering.2019

141. liaiju , WANG Weiqiang  and 李爱菊. Effects of resin content and preparing conditions on the properties of polyphenylene sulfide resin/graphite composite for bipolar plate .JOURNAL OF POWER SOURCES.2008,178 (1):363

142. WANG Weiqiang  and liaiju. The explosion reason analysis of urea reactor of Pingyin .Engineering Failure Analysis.2009,16 (3):972

143. WANG Weiqiang. 平阴尿素合成塔起爆源处层板应力腐蚀开裂分析 .金属热处理.2009,34 (1):104

144. WANG Weiqiang. 尿素合成塔蒸汽爆炸机理及可能断裂过程分析 .全国化工过程机械博士研究生创新研讨会论文摘要集,2009,南京.2009

145. WANG Weiqiang. 尿素合成塔爆炸原因分析研究进展 .全国化工过程机械博士研究生创新研讨会,2009,南京.2009

146. WANG Weiqiang  and 张国新. 自动球压痕法估测Q235B钢的断裂韧度 .机械强度.2018 (05)

147. WANG Weiqiang  and wangshang. 电工层压木静态力学性能测试 .中南林业科技大学学报.2018 (02)

148. WANG Weiqiang  and 张明. 余热锅炉给水泵轴瓦失效分析 .齐鲁工业大学学报.2018 (01)

149. WANG Weiqiang  and 郭建章. 基于均匀设计和BP神经网络的花生油SFE-CO_2萃取预测 .食品科学技术学报.2018 (03)

150. WANG Weiqiang  and 郭建章. 基于均匀设计的SFE-CO_2萃取花生油工艺 .陕西农业科学.2018 (06)

151. WANG Weiqiang  and 牛俊男. 超临界二氧化碳喷染器中平滑式迷宫密封结构对密封性的影响 .润滑与密封.2018 (04)

152. WANG Weiqiang  and wangshang. 最小二乘法估算变压器绝缘件瑞利阻尼系数的可行性研究 .机械科学与技术.2018 (07)

153. WANG Weiqiang , Yanpeng Qu  and 肖克峰. Cefquinome Controlled Size Submicron Particles Precipitation by SEDS Process Using Annular Gap Nozzle .Int. J. Chem. Eng..2017,2017

154. WANG Weiqiang  and 李梦丽. Study on the Microstructure and Mechanical Properties of 20 Steel Strain Aging .PROCEEDINGS OF THE 2017 4TH INTERNATIONAL CONFERENCE ON MACHINERY, MATERIALS AND COMPUTER (MACMC 2017).2017,150 :268

155. WANG Weiqiang  and 张泰瑞. Determination of the proof strength and flow properties of materials from spherical indentation tests: An analytical approach based on the expanding cavity model .JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN.2018,53 (4):225

156. WANG Weiqiang  and 张泰瑞. Improved methods to determine the elastic modulus and area reduction rate in spherical indentation tests .MATERIALS TESTING.2018,60 (4):355

157. WANG Weiqiang  and 张泰瑞. Method to determine the optimal constitutive model from spherical indentation tests .Results in Physics.2018,8 :716

158. WANG Weiqiang  and Xu, Shugen. Numerical investigation of thermo-mechanical stress in U-tube including forming effect for the SCC failure analysis .Engineering Failure Analysis.2017,77 :126

159. WANG Weiqiang , lijianfeng  and 王鹏飞. Research on Fatigue Damage of Compressor Blade Steel KMN-I Using Nonlinear Ultrasonic Testing .Shock and vibration.2017, 0

160. WANG Weiqiang  and 张泰瑞. A constitutive model independent analytical method in determining the tensile properties from incremental spherical indentation tests (ISITs) .International Journal of Mechanical Sciences.2018,148 :9

161. Songying CHEN  and WANG Weiqiang. Numerical simulation of dispersed phase flow in a tube considering bubbles erosion and Cl- ions concentration effects .Advanced Materials research.2011,314-316 (0):1069

162. yumeijie  and WANG Weiqiang. 聚丙烯腈预氧丝皮芯结构的影响因素与防控措施. .《功能材料》.2010,41 (6):1019

163. WANG Weiqiang  and lijianfeng. Fatigue behavior and mechanism of FV520B-I welding seams in a very high cycle regime .International Journal of Fatigue.2016,87 :22

164. liaiju , WANG Weiqiang  and 李爱菊. 树脂/石墨PEMFC双极板的制备工艺与性能研究综述 .《材料导报》.2013,27 (9):87

165. wangchengguo , WANG Weiqiang  and yumeijie. Thermal Properties of Acrylonitrile/Itaconic Acid Polymers in Oxidative and Nonoxidative Atmospheres .Journal of applied polymer science.2010,116 (2):1207

166. Yanpeng Qu  and WANG Weiqiang. The structural design of nozzle in outer mixing mode for preparing superfine particles by SCF technology .Advanced Materials Research .2011

167. WANG Weiqiang  and 杨炎. 服役后16Mn管材应变时效的自动球压痕测试 .山东大学学报(工学版).2017,47 (04):64

168. WANG Weiqiang  and 张泰瑞. A unified energy release rate based model to determine the fracture toughness of ductile metals from unnotched specimens .INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES Journal.2019,150 :35

169. WANG Weiqiang , lijianfeng  and 王鹏飞. Fatigue behavior and mechanism of KMN in a very high cycle regime .MATERIALS TESTING.2018,60 (1):55

170. Yanpeng Qu  and WANG Weiqiang. 超临界流体多过程试验平台研究 .2014

171. WANG Weiqiang. 尿素合成塔液相泄漏蒸气爆炸压力计算 .化肥工业.2012,39 (2)

172. WANG Weiqiang  and Yanpeng Qu. 用于超临界流体工艺过程的板式换热器 .2012

173. WANG Weiqiang  and Yanpeng Qu. 超临界流体技术制备超微粉体用径向组合型喷嘴 .2010

174. WANG Weiqiang. FAULT TREE ANALYSIS ON SEAL FAILURE OF HIGH PRESSURE AMMONIUM CARBAMATE PUMP .2008

175. WANG Weiqiang. 基于ANSYS Workbench和FLUENT的超临界二氧化碳萃取釜流场模拟及其结构改进 .《化工进展》.2012,31 (9):1914

176. WANG Weiqiang. 奥氏体不锈钢换热管应力腐蚀开裂分析 .《化工机械》.2012

177. WANG Weiqiang. 局部冲击压力下多层包扎容器弹性动力响应分析 .石油化工设备.2012,41 (3):34

178. WANG Weiqiang. 活塞式压缩机联轴器连接螺栓断裂原因分析 .理化检验-物理分册.2012,48 (3):203

179. WANG Weiqiang. 尿素合成塔爆炸载荷类型与破坏形态的关系分析 .山东大学学报(工学版).2008,38 (3):51

180. WANG Weiqiang. 磁致伸缩导波技术检测管道缺陷 .《无损检测》.2008,30 (7):434

181. WANG Weiqiang. 多层包扎尿素合成塔应力状况分析 .机械强度.2008,30 (1):93

182. WANG Weiqiang. WNN优化模型在模拟超临界二氧化碳中固体溶解度的应用 .天然气化工(C1化学与化工).2008,33 (3):75

183. WANG Weiqiang. 平阴尿塔的物料和爆炸能量估算 .山东大学学报(工学版).2008,38 (3):46

184. WANG Weiqiang. Urea reactor integrity evaluation based on failure analysis .Journal of Pressure Vessel Technology, Transa.2007,v 129 (n 4):744

185. WANG Weiqiang. 氨合成废热锅炉换热管应力腐蚀开裂分析 .《压力容器》.2008,25 (3):41

186. WANG Weiqiang  and 李爱菊. 聚苯硫醚/石墨基双极板复合材料性能的研究 .《人工晶体学报》.2008,37 (4):819

187. WANG Weiqiang. Structural and Regulating Characteristics of Adjustable Annulus-clearance Nozzle Used in Supercritical Fluid Precipitation .武汉理工大学学报(材料科学版)(英文版).2017,32 (6):1487

188. Yanpeng Qu , liaiju  and WANG Weiqiang. Structural and regulating characteristics of adjustable annulus-clearance nozzle used in supercritical fluid precipitation . Journal Wuhan University of Technology, Materials Science Edition.2017,32 (6):1487

189. WANG Weiqiang. 尿素合成塔层板严重腐蚀开裂分析 .2008

190. WANG Weiqiang. 磁致伸缩导波技术在构件腐蚀检测中的应用实践 .无损探伤.2008,2008年卷 (5):18

191. WANG Weiqiang. 水溶液全循环尿素生产装置中静设备失效类型和机理研究 .2008

192. WANG Weiqiang. 疲劳概率模型的综合评价方法 .中国机械工程.2008,19 (23):2812

193. WANG Weiqiang. 平阴尿塔塔体爆炸能量分析与计算 .山东大学学报(工学版).2008,38 (4):80

194. WANG Weiqiang. 合成氨装置风险预测控制系统的研究 .2008

195. WANG Weiqiang. 尿素合成塔物料蒸气爆炸初步研究 .2008

196. WANG Weiqiang. Catastrophic Explosion of a Multilayered Urea Reactor .2008

197. WANG Weiqiang. Application of the Analytic Hierarchy Process in Risk Analysis for Urea Reactor .2008

198. WANG Weiqiang. 尿素合成塔风险分析 .腐蚀科学与防护技术.2008,20 (5):377

199. WANG Weiqiang. 尿素合成塔层板开裂规律及原因分析 .2009

200. WANG Weiqiang. 锅炉水冷壁管腐蚀爆裂失效分析 .2013

201. WANG Weiqiang. Failure analysis of spiral plate heat exchanger .2011

202. WANG Weiqiang. Failure analysis of 20G boiler tubes .2010

203. WANG Weiqiang. Root cause analysis of stress corrosion at tube-to-tubesheet joints of a waste heat boiler .Engineering Failure Analysis.2014,45 :398

204. Yanpeng Qu  and WANG Weiqiang. 超临界流体喷染的原理及研究进展 .2014

205. WANG Weiqiang. Research on the properties of 20G steel with strain aging embrittlement using indentation test .2012

206. WANG Weiqiang. The pressure variation of BLEVE triggered by liquid release through a crack in the cylindrical pressure vessel .2012

207. WANG Weiqiang. Preparation of ultra-fine powder using supercritical fluids: A review .2011

208. WANG Weiqiang. The stress corrosion cracking of austenitic stainless steel heat exchange tubes—three cases study .2010

209. WANG Weiqiang. Using FEM to predict residual stresses in girth welding joint of layered cylindrical vessels .International Journal of Pressure Vessels and Piping.2014,119 :1

210. lijianfeng  and WANG Weiqiang. Fatigue behavior and mechanism of FV520B-I in ultrahigh cycle regime .2014

211. WANG Weiqiang. Residual stresses in the welding joint of the nozzle-to-head area of a layered high-pressure hydrogen storage tank .International journal of hydrogen energy.2014,39 (21):11061

212. WANG Weiqiang. On-Line monitoring method for centrifugal compressor and impeller remanufacturing .2012

213. WANG Weiqiang. Failure analysis of a bellows expansion joint of inconel625 alloy .2012

214. WANG Weiqiang. 甲胺反应器严重开裂原因分析. .2009

215. liaiju  and WANG Weiqiang. The stress distribution and critical c rack length analysis of a cracked multilayer urea reactor .2012

216. WANG Weiqiang. 20(G)板不同焊接缺陷的磁记忆信号检测分析 .中国特种设备安全.2016,32 (5):33

217. WANG Weiqiang. A New Method to the Elastodynamic Response of a Spherical Shell Under the Impact Load .Journal of Pressure Vessel Technology.2016,138 (3):345011

218. WANG Weiqiang. The Measurement of Mechanical Properties of Pipe Steels in Service through Continuous Ball Indentation Test .2015

219. WANG Weiqiang. 水冷壁管开裂原因分析 .化工装备.2015 (2):37

220. WANG Weiqiang. 连续球压痕法测试压力容器钢力学性能的研究 .振动.测试与诊断.2015,35 (2):281

221. WANG Weiqiang. Failure analysis of stress corrosion cracking in heat exchanger tubes during start-up operation .Engineering Failure Analysis.2015,51 :1

222. WANG Weiqiang. Mathematical model for tension of textile during the process of supercritical fluids spray dyeing .2014

223. WANG Weiqiang. 法兰密封系统应力松弛有限元分析 .《压力容器》.2013,30 (4):23

224. WANG Weiqiang. Study on the strength of textile during the process of supercritical fluids spray dyeing .2014

225. WANG Weiqiang. SCF preparation of drug particle using size adjustable nozzle .2012

226. Yanpeng Qu , Songying CHEN  and WANG Weiqiang. Significance analysis on influential factors of stress corrosion based on grey relational theory for stainless steels .2012

227. WANG Weiqiang. The feasibility of research for shell deformations with isogeometric analysis .2012

228. WANG Weiqiang. Failure analysis of the pure zirconium hanging sample for acetic anhydride reactor .2012

229. WANG Weiqiang. Numerical investigation on weld residual stresses in tube to tube sheet joint of a heat exchanger .International Journal of Pressure Vessels and Piping.2013,101 :37

230. WANG Weiqiang , sunjie  and lijianfeng. Effect of cracked blade distribution on strength of centrifugal impeller .2013

231. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on developed solution structure theorem for wave equation .Journal of Pressure Vessel Technology, Transactions of the ASME.2011,134 (1):112101

232. WANG Weiqiang. Analysis on elastoplastic stress distribution in a layered cylindrical vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transactions of the ASME.2012,134 (3):312061

233. Yanpeng Qu  and WANG Weiqiang. Supercritical fluid pray dyeing: A new method of dyeing and simulations of its flow field. .2011

234. WANG Weiqiang. The exploration of strain aging embrittlement evaluation in metallic materials using indentation test .2011

235. WANG Weiqiang. Grey predication of corrosion on oil atmospheric distillation equipment .2009

236. WANG Weiqiang. Grey decision on oil distillation tower top exchangers maintenance overhaul .2009

237. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on generalized solution structure theorem for wave equation .2010

238. WANG Weiqiang. Modified formulation of layer stresses due to Internal pressure of a layered vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transa.2010,132 (5):5120101

239. WANG Weiqiang. A Fortran implementation of isogeometric analysis with superiority in convergence and accuracy .2015

240. WANG Weiqiang , LI Fangyi , lijianfeng  and Lester. Damage mechanism and evaluation model of compressor impeller remanufacturing blanks: A review .Frontiers of Mechanical Engineering.2019

241. WANG Weiqiang  and 李爱菊. Effects of resin content and preparing conditions on the properties of polyphenylene sulfide resin/graphite composite for bipolar plate .JOURNAL OF POWER SOURCES.2008,178 (1):363

242. WANG Weiqiang. 平阴尿素合成塔起爆源处层板应力腐蚀开裂分析 .金属热处理.2009,34 (1):104

243. WANG Weiqiang. 尿素合成塔蒸汽爆炸机理及可能断裂过程分析 .2009

244. WANG Weiqiang. 尿素合成塔爆炸原因分析研究进展 .2009

245. WANG Weiqiang  and Songying CHEN. Numerical simulation of dispersed phase flow in a tube considering bubbles erosion and Cl- ions concentration effects .Advanced Materials research.2011,314-316 (0):1069

246. WANG Weiqiang  and yumeijie. 聚丙烯腈预氧丝皮芯结构的影响因素与防控措施. .《功能材料》.2010,41 (6):1019

247. WANG Weiqiang  and 李爱菊. 树脂/石墨PEMFC双极板的制备工艺与性能研究综述 .《材料导报》.2013,27 (9):87

248. wangchengguo , WANG Weiqiang  and yumeijie. Thermal Properties of Acrylonitrile/Itaconic Acid Polymers in Oxidative and Nonoxidative Atmospheres .Journal of applied polymer science.2010,116 (2):1207

249. WANG Weiqiang  and 李爱菊. 聚苯硫醚/石墨基双极板复合材料性能的研究 .《人工晶体学报》.2008,37 (4):819

250. Yanpeng Qu , liaiju  and WANG Weiqiang. Structural and regulating characteristics of adjustable annulus-clearance nozzle used in supercritical fluid precipitation . Journal Wuhan University of Technology, Materials Science Edition.2017,32 (6):1487

251. liaiju , Yanpeng Qu  and WANG Weiqiang. 超临界流体多工艺过程试验平台的模块化设计 .2012

252. Yanpeng Qu  and WANG Weiqiang. 超临界流体技术制备超微粉体喷嘴结构设计 .2007

253. WANG Weiqiang. 局部冲击压力下多层包扎容器弹性动力响应分析 .石油化工设备.2012,41 (3):34

254. WANG Weiqiang. 活塞式压缩机联轴器连接螺栓断裂原因分析 .理化检验-物理分册.2012,48 (3):203

255. WANG Weiqiang. Structural and Regulating Characteristics of Adjustable Annulus-clearance Nozzle Used in Supercritical Fluid Precipitation .武汉理工大学学报(材料科学版)(英文版).2017,32 (6):1487

256. WANG Weiqiang  and 李爱菊. Effects of resin content and preparing conditions on the properties of polyphenylene sulfide resin/graphite composite for bipolar plate .JOURNAL OF POWER SOURCES.2008,178 (1):363

257. Yanpeng Qu , liaiju  and WANG Weiqiang. 超臨界流體噴染及其流場數值模擬研究 .2012

258. Yanpeng Qu  and WANG Weiqiang. 超临界流体多过程试验平台研究 .2014

259. WANG Weiqiang  and Yanpeng Qu. Novel Multi-Stream Plate Exchanger under High Pressure—Structure and its Design Method .Advanced Materials research.2014,1062 :658

260. WANG Weiqiang. 尿素合成塔液相泄漏蒸气爆炸压力计算 .化肥工业.2012,39 (2)

261. WANG Weiqiang. 尿素合成塔爆破原因分析综述 .机械强度.2012,34 (3):427

262. WANG Weiqiang  and Yanpeng Qu. 用于超临界流体工艺过程的板式换热器 .2012

263. WANG Weiqiang  and Yanpeng Qu. 超临界流体技术制备超微粉体用径向组合型喷嘴 .2010

264. WANG Weiqiang. FAULT TREE ANALYSIS ON SEAL FAILURE OF HIGH PRESSURE AMMONIUM CARBAMATE PUMP .2008

265. WANG Weiqiang , liaiju  and Yanpeng Qu. SCF快速膨胀过程流动模拟及其工艺参数的影响 .2008

266. WANG Weiqiang. 基于ANSYS Workbench和FLUENT的超临界二氧化碳萃取釜流场模拟及其结构改进 .《化工进展》.2012,31 (9):1914

267. WANG Weiqiang , liaiju  and Yanpeng Qu. 喷嘴和结晶器结构及参数对SAS法制备超微粉体的影响 .2009

268. WANG Weiqiang. 奥氏体不锈钢换热管应力腐蚀开裂分析 .《化工机械》.2012

269. lijianfeng  and WANG Weiqiang. Fatigue behavior and mechanism of FV520B-I welding seams in a very high cycle regime .International Journal of Fatigue.2016,87 :22

270. WANG Weiqiang  and Yanpeng Qu. The structural design of nozzle in outer mixing mode for preparing superfine particles by SCF technology .2011

271. WANG Weiqiang. 超临界流体技术制备超微粉体的新型喷嘴 .《化工机械》.2008,35 (6):374

272. WANG Weiqiang. 尿素合成塔爆炸载荷类型与破坏形态的关系分析 .山东大学学报(工学版).2008,38 (3):51

273. WANG Weiqiang. 磁致伸缩导波技术检测管道缺陷 .《无损检测》.2008,30 (7):434

274. WANG Weiqiang. 多层包扎尿素合成塔应力状况分析 .机械强度.2008,30 (1):93

275. WANG Weiqiang. WNN优化模型在模拟超临界二氧化碳中固体溶解度的应用 .天然气化工(C1化学与化工).2008,33 (3):75

276. WANG Weiqiang. 平阴尿塔的物料和爆炸能量估算 .山东大学学报(工学版).2008,38 (3):46

277. Yanpeng Qu  and WANG Weiqiang. 新型超临界流体染色器设计 .2008

278. WANG Weiqiang. Urea reactor integrity evaluation based on failure analysis .Journal of Pressure Vessel Technology, Transa.2007,v 129 (n 4):744

279. WANG Weiqiang. 氨合成废热锅炉换热管应力腐蚀开裂分析 .《压力容器》.2008,25 (3):41

280. WANG Weiqiang. 尿素合成塔层板严重腐蚀开裂分析 .2008

281. WANG Weiqiang. 磁致伸缩导波技术在构件腐蚀检测中的应用实践 .无损探伤.2008,2008年卷 (5):18

282. WANG Weiqiang. 水溶液全循环尿素生产装置中静设备失效类型和机理研究 .2008

283. WANG Weiqiang. 疲劳概率模型的综合评价方法 .中国机械工程.2008,19 (23):2812

284. WANG Weiqiang. 平阴尿塔塔体爆炸能量分析与计算 .山东大学学报(工学版).2008,38 (4):80

285. WANG Weiqiang. 合成氨装置风险预测控制系统的研究 .2008

286. WANG Weiqiang. 尿素合成塔物料蒸气爆炸初步研究 .2008

287. WANG Weiqiang. 锅炉汽包至上集箱间联络管爆破原因分析 .《压力容器》.2008,25 (10):33

288. zhanglewen  and WANG Weiqiang. FEM analyses of stress and deformation of a flexible inner pressure bolt .Journal of China University of Mining and Tec.2008,18 (4):584

289. WANG Weiqiang. Catastrophic Explosion of a Multilayered Urea Reactor .2008

290. WANG Weiqiang. Application of the Analytic Hierarchy Process in Risk Analysis for Urea Reactor .2008

291. WANG Weiqiang. 尿素合成塔风险分析 .腐蚀科学与防护技术.2008,20 (5):377

292. WANG Weiqiang. 尿素合成塔层板开裂规律及原因分析 .2009

293. WANG Weiqiang. 锅炉水冷壁管腐蚀爆裂失效分析 .2013

294. WANG Weiqiang , sunjie  and lijianfeng. Effect of cracked blade distribution on vibration characteristics of centrifugal impeller .2013

295. WANG Weiqiang. Failure analysis of spiral plate heat exchanger .2011

296. liaiju  and WANG Weiqiang. Study on the microstructure of 20 steel with strain aging .2011

297. WANG Weiqiang. Failure analysis of 20G boiler tubes .2010

298. liaiju  and WANG Weiqiang. 避免Q245钢厚壁高压管应变时效脆化的试验研究 .2009

299. WANG Weiqiang. Root cause analysis of stress corrosion at tube-to-tubesheet joints of a waste heat boiler .Engineering Failure Analysis.2014,45 :398

300. WANG Weiqiang. 通过标准规避高压钢管应变时效脆化的发生 .《压力容器》.2010,27 (11):45

301. Yanpeng Qu  and WANG Weiqiang. 超临界流体喷染的原理及研究进展 .2014

302. WANG Weiqiang. Research on the properties of 20G steel with strain aging embrittlement using indentation test .2012

303. WANG Weiqiang. The pressure variation of BLEVE triggered by liquid release through a crack in the cylindrical pressure vessel .2012

304. wangyanming , liaiju  and WANG Weiqiang. Effect of fiber surface treatment techniques on properties of short carbon fiber reinforced phenol formaldehyde resin/graphite composite bipolar plate .2011

305. WANG Weiqiang. Preparation of ultra-fine powder using supercritical fluids: A review .2011

306. liaiju  and WANG Weiqiang. 消除Q245钢应变时效脆化的理论分析及试验研究 .2009

307. WANG Weiqiang. The stress corrosion cracking of austenitic stainless steel heat exchange tubes—three cases study .2010

308. liaiju  and WANG Weiqiang. The Fracture Failure Analysis of a Hot Pure Water Storage Container .2015

309. Yanpeng Qu  and WANG Weiqiang. Effects of austenitic stainless steel tube and tubesheet hole dimensional deviations on the hydraulic expansion pressure .International Journal of Pressure Vessels and Piping.2016,138 :1

310. Yanpeng Qu  and WANG Weiqiang. A Fortran implementation of isogeometric analysis for thin plate problems with the penalty method .Engineering Computations.2016,33 (7):2149

311. WANG Weiqiang. Using FEM to predict residual stresses in girth welding joint of layered cylindrical vessels .International Journal of Pressure Vessels and Piping.2014,119 :1

312. lijianfeng  and WANG Weiqiang. Fatigue behavior and mechanism of FV520B-I in ultrahigh cycle regime .2014

313. WANG Weiqiang. Residual stresses in the welding joint of the nozzle-to-head area of a layered high-pressure hydrogen storage tank .International journal of hydrogen energy.2014,39 (21):11061

314. WANG Weiqiang. On-Line monitoring method for centrifugal compressor and impeller remanufacturing .2012

315. WANG Weiqiang. Failure analysis of a bellows expansion joint of inconel625 alloy .2012

316. WANG Weiqiang. 甲胺反应器严重开裂原因分析. .2009

317. liaiju  and WANG Weiqiang. Study on the Brittle Fracture of the Q245 Steel High Pressure Piping in an Ammonia Synthesis Unit .2009

318. liaiju  and WANG Weiqiang. Analysis on layer cracking of urea reactors .2010

319. liaiju  and WANG Weiqiang. The stress distribution and critical c rack length analysis of a cracked multilayer urea reactor .2012

320. Yanpeng Qu  and WANG Weiqiang. 重整氢压缩机连杆螺栓断裂失效分析 .金属热处理.2016,41 (2):200

321. WANG Weiqiang. 20(G)板不同焊接缺陷的磁记忆信号检测分析 .中国特种设备安全.2016,32 (5):33

322. Yanpeng Qu  and WANG Weiqiang. 基于场协同原理的管道经济管径计算新方法 .流体机械.2016,44 (8):32

323. WANG Weiqiang. A New Method to the Elastodynamic Response of a Spherical Shell Under the Impact Load .Journal of Pressure Vessel Technology.2016,138 (3):345011

324. Yanpeng Qu  and WANG Weiqiang. Probability Analysis of Pit Initiation on Austenitic Stainless Steels .2015

325. WANG Weiqiang. The Measurement of Mechanical Properties of Pipe Steels in Service through Continuous Ball Indentation Test .2015

326. Yanpeng Qu  and WANG Weiqiang. Failure analysis of austenitic stainless pipes in amine liquid regeneration unit of a desulfurizer .Engineering Failure Analysis.2015,57 :164

327. WANG Weiqiang. 水冷壁管开裂原因分析 .化工装备.2015 (2):37

328. WANG Weiqiang. 连续球压痕法测试压力容器钢力学性能的研究 .振动.测试与诊断.2015,35 (2):281

329. WANG Weiqiang. Failure analysis of stress corrosion cracking in heat exchanger tubes during start-up operation .Engineering Failure Analysis.2015,51 :1

330. lijianfeng  and WANG Weiqiang. Fatigue behavior and mechanism of FV520B in very high cycle regime .Strength, Fracture and Complexity.2015,9 (2):161

331. WANG Weiqiang. Mathematical model for tension of textile during the process of supercritical fluids spray dyeing .2014

332. WANG Weiqiang. 法兰密封系统应力松弛有限元分析 .《压力容器》.2013,30 (4):23

333. WANG Weiqiang. Study on the strength of textile during the process of supercritical fluids spray dyeing .2014

334. WANG Weiqiang. SCF preparation of drug particle using size adjustable nozzle .2012

335. Yanpeng Qu , Songying CHEN  and WANG Weiqiang. Significance analysis on influential factors of stress corrosion based on grey relational theory for stainless steels .2012

336. WANG Weiqiang. The feasibility of research for shell deformations with isogeometric analysis .2012

337. WANG Weiqiang. Failure analysis of the pure zirconium hanging sample for acetic anhydride reactor .2012

338. WANG Weiqiang. Numerical investigation on weld residual stresses in tube to tube sheet joint of a heat exchanger .International Journal of Pressure Vessels and Piping.2013,101 :37

339. WANG Weiqiang , sunjie  and lijianfeng. Effect of cracked blade distribution on strength of centrifugal impeller .2013

340. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on developed solution structure theorem for wave equation .Journal of Pressure Vessel Technology, Transactions of the ASME.2011,134 (1):112101

341. WANG Weiqiang. Analysis on elastoplastic stress distribution in a layered cylindrical vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transactions of the ASME.2012,134 (3):312061

342. WANG Weiqiang. Solution of gas explosion load and simulation of dynamic response of multilayer structures .2012

343. Yanpeng Qu  and WANG Weiqiang. Supercritical fluid pray dyeing: A new method of dyeing and simulations of its flow field. .2011

344. liaiju  and WANG Weiqiang. 热处理避免和消除20钢厚壁高压管应变时效脆化实验研究 .《材料工程》.2011,2011年卷 (1):57

345. Yanpeng Qu , guancongsheng  and WANG Weiqiang. 管壳式固定床反应器爆炸事故分析 .《化工机械》.2010,37 (2):222

346. WANG Weiqiang. 我国特种设备事故调查与处理体制的思考 .中国特种设备安全.2010,2010年卷 (7):33

347. liaiju  and WANG Weiqiang. A simplification method of defects in multilayered vessels detected by acoustic emission detection .2009

348. WANG Weiqiang. The exploration of strain aging embrittlement evaluation in metallic materials using indentation test .2011

349. liaiju  and WANG Weiqiang. Study on the composites of phenol formaldehyde resin/graphite reinforced by milled carbon fibers for bipolar plates .2010

350. WANG Weiqiang. Grey predication of corrosion on oil atmospheric distillation equipment .2009

351. Yanpeng Qu  and WANG Weiqiang. Preparation of Cefquinome Nanoparticles by Using the Supercritical Antisolvent Process .Journal of Nanomaterials.2015,2015(ID: 767945 ) :1

352. liaiju  and WANG Weiqiang. Failure analysis of the brittle fracture of thick-walled 20 steel pipe in an ammonia synthesis unit .Engineering Failure Analysis.2010,17 (6):1359

353. WANG Weiqiang. 我国高压管道标准中某些规定存在的问题与思考 .2010

354. WANG Weiqiang. Grey decision on oil distillation tower top exchangers maintenance overhaul .2009

355. lijianfeng  and WANG Weiqiang. 连续球压痕测定常用叶轮材料力学性能的研究 .流体机械.2015,43 (2):7

356. WANG Weiqiang. A new approach to elastodynamic response of cylindrical shell based on generalized solution structure theorem for wave equation .2010

357. WANG Weiqiang. Modified formulation of layer stresses due to Internal pressure of a layered vessel with interlayer gaps .Journal of Pressure Vessel Technology, Transa.2010,132 (5):5120101

358. WANG Weiqiang. A Fortran implementation of isogeometric analysis with superiority in convergence and accuracy .2015

359. Yanpeng Qu  and WANG Weiqiang. 超临界流体染纱器现状与新型结构 .《现代化工》.2010,30 (7):65

360. liaiju  and WANG Weiqiang. The explosion reason analysis of urea reactor of Pingyin .Engineering Failure Analysis.2009,16 (3):972

361. WANG Weiqiang. 平阴尿素合成塔起爆源处层板应力腐蚀开裂分析 .金属热处理.2009,34 (1):104

362. WANG Weiqiang. 尿素合成塔蒸汽爆炸机理及可能断裂过程分析 .2009

363. WANG Weiqiang. 尿素合成塔爆炸原因分析研究进展 .2009

364. WANG Weiqiang , Yanpeng Qu  and 肖克峰. Cefquinome Controlled Size Submicron Particles Precipitation by SEDS Process Using Annular Gap Nozzle .Int. J. Chem. Eng..2017,2017

365. WANG Weiqiang  and 李梦丽. Study on the Microstructure and Mechanical Properties of 20 Steel Strain Aging .PROCEEDINGS OF THE 2017 4TH INTERNATIONAL CONFERENCE ON MACHINERY, MATERIALS AND COMPUTER (MACMC 2017).2017,150 :268

366. WANG Weiqiang  and 苏成功. 压痕对不锈钢材料表面残余应力的影响 .山东大学学报(工学版).2017,47 (01):90

367. WANG Weiqiang  and Xu, Shugen. Numerical investigation of thermo-mechanical stress in U-tube including forming effect for the SCC failure analysis .Engineering Failure Analysis.2017,77 :126

368. WANG Weiqiang , lijianfeng  and 王鹏飞. Research on Fatigue Damage of Compressor Blade Steel KMN-I Using Nonlinear Ultrasonic Testing .Shock and vibration.2017, 0

369. WANG Weiqiang  and 杨炎. 服役后16Mn管材应变时效的自动球压痕测试 .山东大学学报(工学版).2017,47 (04):64

370. WANG Weiqiang  and 张泰瑞. A unified energy release rate based model to determine the fracture toughness of ductile metals from unnotched specimens .INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES Journal.2019,150 :35

371. wangchengguo , WANG Weiqiang  and yumeijie. Thermal Properties of Acrylonitrile/Itaconic Acid Polymers in Oxidative and Nonoxidative Atmospheres .Journal of applied polymer science.2010,116 (2):1207

372. Yanpeng Qu , WANG Weiqiang  and 刘燕. The structural design of nozzle in outer mixing mode for preparing superfine particles by SCF technology .Advanced Materials research.2011

373. WANG Weiqiang  and 李爱菊. 树脂/石墨PEMFC双极板的制备工艺与性能研究综述 .《材料导报》.2013,27 (9):87

374. Yanpeng Qu , WANG Weiqiang  and 刘燕. Non-dimensional Design Method for Pressure Vessels. .Advanced Materials Research ,Advanced Mechanical Design.2012,Vols. 479-481 (2012) :1704

375. WANG Weiqiang  and 张泰瑞. Method to determine the optimal constitutive model from spherical indentation tests .Results in Physics.2018,8 :716

376. WANG Weiqiang  and 张泰瑞. Improved methods to determine the elastic modulus and area reduction rate in spherical indentation tests .MATERIALS TESTING.2018,60 (4):355

377. WANG Weiqiang  and 郭建章. 基于均匀设计的SFE-CO_2萃取花生油工艺 .陕西农业科学.2018 (06)

378. WANG Weiqiang  and 郭建章. 基于均匀设计和BP神经网络的花生油SFE-CO_2萃取预测 .食品科学技术学报.2018 (03)

379. WANG Weiqiang  and wangshang. 最小二乘法估算变压器绝缘件瑞利阻尼系数的可行性研究 .机械科学与技术.2018 (07)

380. WANG Weiqiang  and wangshang. 电工层压木静态力学性能测试 .中南林业科技大学学报.2018 (02)

381. WANG Weiqiang  and 张明. 余热锅炉给水泵轴瓦失效分析 .齐鲁工业大学学报.2018 (01)

382. WANG Weiqiang  and 张泰瑞. Determination of the proof strength and flow properties of materials from spherical indentation tests: An analytical approach based on the expanding cavity model .JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN.2018,53 (4):225

383. WANG Weiqiang  and 张泰瑞. A constitutive model independent analytical method in determining the tensile properties from incremental spherical indentation tests (ISITs) .International Journal of Mechanical Sciences.2018,148 :9

384. WANG Weiqiang  and Songying CHEN. Numerical simulation of dispersed phase flow in a tube considering bubbles erosion and Cl- ions concentration effects .Advanced Materials research.2011,314-316 (0):1069

385. WANG Weiqiang , lijianfeng  and 刘燕. Fatigue behavior and mechanism of FV520B-I welding seams in a very high cycle regime .International Journal of Fatigue.2016,87 :22

386. WANG Weiqiang  and yumeijie. 聚丙烯腈预氧丝皮芯结构的影响因素与防控措施. .《功能材料》.2010,41 (6):1019

387. WANG Weiqiang  and 张国新. 自动球压痕法估测Q235B钢的断裂韧度 .机械强度.2018 (05)

388. WANG Weiqiang  and 牛俊男. 超临界二氧化碳喷染器中平滑式迷宫密封结构对密封性的影响 .润滑与密封.2018 (04)

389. WANG Weiqiang , lijianfeng  and 王鹏飞. Fatigue behavior and mechanism of KMN in a very high cycle regime .MATERIALS TESTING.2018,60 (1):55

Patens

1. 一种基于双极性磁卡材料的磁制冷装置及方法

2. 一种变壁厚连萃器筒体以及连萃器

3. 一种压力逐级升降自平衡的高压或超高压阀门切换系统

4. 一种高压或超高压套管换热器

5. 一种收放式超临界流体对喷染色器及对喷染色工艺

6. 一种旋转式超临界流体对喷染色器及对喷染色工艺

7. 一种含商陆的复方植物杀虫剂

8. 超临界流体萃取制备植物源农药的方法

9. 超临界流体纳微米材料制备用精调环隙组合喷嘴

10. 一种可移动筒体的压力容器快开装置

11. 超临界流体连续染纱器

12. 超临界流体连续萃取装置

13. 一种树脂/石墨复合材料双极板连续成形装置及制备工艺

14. 外混式超临界流体纳微材料制备喷嘴

15. 内混式超临界流体纳微材料制备喷嘴

16. 一种蒸汽检漏系统及检漏介质参数

17. 膨胀锚杆

18. 复合塑料船艇体及其模压成型方法

19. 环向限延伸柔性注压锚杆

20. 厚涂层附着力检测方法及检测装置

21. 超临界流体喷染装置

22. 结合尿素生产系统的超临界二氧化碳染色工艺流程

23. 一种超临界流体制备纳微米材料的外部可调径向扩展环隙组合喷嘴

24. 内外混式超临界流体纳微材料制备喷嘴

25. 一种磨碎碳纤维增强的酚醛树脂/石墨双极板材料

26. 一种真空检漏系统

27. ?高压超高压连续固体物料萃取和灭菌装置

28. 一种磨碎碳纤维增强树脂\石墨导电复合材料及其制备工艺

29. 一种超临界流体卷染工艺

30. 超临界流体对喷染色设备

31. 超临界流体连续浸染设备

32. 一种从番茄中萃取分离番茄红素的方法

33. 超临界流体喷染装置

34. 结合尿素生产系统的超临界二氧化碳染色工艺流程

35. 一种真空检漏系统

36. 一种磨碎碳纤维增强的酚醛树脂/石墨双极板材料

37. ?高压超高压连续固体物料萃取和灭菌装置

38. 一种磨碎碳纤维增强树脂\石墨导电复合材料及其制备工艺

39. 高压超高压介质环境屏蔽电机

40. 一种超临界流体卷染工艺

41. 超临界流体对喷染色设备

42. 超临界流体连续浸染设备

43. 内外混式超临界流体纳微材料制备喷嘴

44.  高压超高压连续固体物料萃取和灭菌装置

45. 超临界流体喷染装置

46. 结合尿素生产系统的超临界二氧化碳染色工艺流程

47. 超临界流体连续萃取装置

48. 高压超高压介质环境屏蔽电机

49. 一种新型超临界流体喷染用喷射器

50. 一种超临界流体喷染用喷射器

51. 一种树脂/石墨复合材料双极板连续成形装置及制备工艺

52. 一种可移动筒体的压力容器快开装置

Research project

1. 余热锅炉炉管与管板连接处泄漏的分析及预防方法, 2021/06/10-2022/06/09

2. 仪器化压痕技术评估构件力学性能研究, 2021/07/25-2022/07/24

3. 齐鲁石化热电厂二号汽轮机27Cr2Mo1V转子轴疲劳寿命评估, 2020/12/10-2021/12/31

4. 齐鲁石化热电厂五号汽轮机30Cr1Mo1V转 子轴疲劳与断裂分析, 2021/03/19-2021/12/31

5. 高压屏蔽搅拌釜研究开发, 2020/11/12-2021/11/12

6. 亚临界二氧化碳等压连续萃取分离装置开发, 2020/05/01-2023/05/01

7. 超临界流体(无水)染色装置研制, 2007/01/25-2009/01/25

8. 设备失效分析, 2014/07/07-2018/07/07

9. 再制造对象的多强场、跨尺度损伤行为与机理,可再制造的临界阈值, 2011/11/01-2015/12/31

10. 冲蚀环境下离心压缩机叶轮材料FV520B-I超高周疲劳行为与寿命预测研究, 2017/09/01-2020/12/31

11. 锅炉吊管开裂原因分析, 2018/05/27-2019/05/26

12. 齐鲁石化热电厂一号汽轮机27Cr2Mo1V转子轴疲劳寿命评估, 2018/02/01-2018/12/20

13. 换热器失效分析, 2018/03/18-2019/03/17

14. 可调环隙喷嘴超临界流体制备纳微米材料装置研制, 2017/11/28-2020/11/17

15. 芝麻核桃深加工技术合作开发, 2017/06/18-2022/06/17

16. 在线压痕试验机研制及材料性能测试研究与应用, 2016/07/01-2019/12/31

17. 炉气净化热风炉过滤器水样和管道锈样检测及腐蚀原因分析, 2016/11/03-2017/02/28

18. 超临界二氧化碳喷染机理及连续化装置研究, 2016/08/17-2020/12/31

19. 齐鲁石化热电厂七号汽轮机30Cr1Mo1V转子轴疲劳断裂分析, 2016/06/20-2016/12/20

20. 超临界二氧化碳卷染装置研制, 2016/05/16-2019/05/16

21. 炉管超温材料分析研究, 2016/04/01-2016/12/31

22. 变压器运输加速度与器身绝缘性能关系研究, 2016/01/05-2017/03/31

23. Z41T-10 DN200闸阀阀盖开裂原因分析, 2015/12/31-2016/06/23

24. 汽化炉炉壁复合钢板内层开裂原因分析, 2014/11/22-2015/05/31

25. 自动球压痕法测试材料力学性能的机理和普适性研究, 2014/08/15-2018/12/31

26. 超临界流体多工艺过程综合实验平台的开发, 2014/09/27-2017/09/26

27. 热纯水储罐罐体材料分析, 2014/07/07-2015/07/07

28. 双氧水厂氢化塔板材分析, 2014/05/19-2015/05/19

29. 超临界流体连续萃取装置(山东省), 2013/12/01-2014/12/31

30. 复杂腐蚀环境承压设备的材料选择、结构优化、焊接工艺筛选及热处理优化技术, 2010/09/01-2011/08/31

31. 合成氨与尿素装置基于风险检验技术研究及应用, 2007/08/10-2008/12/30

32. 化工与石油化工装置风险评估与基于风险检验技术研究, 2006/12/10-2008/12/30

33. 层板包扎高压容器(863配套资金), 2006/12/11-2008/12/30

34. 4#3D22氮氢气压缩机失效分析, 2013/01/15-2013/12/31

35. 尿素合成塔(NR-6)材料性能测试分析, 2013/02/15-2013/12/31

36. 设备失效分析, 2012/11/20-2012/12/31

37. 热能分部1#、3#240T锅炉水冷壁管腐蚀爆裂失效原因分析, 2012/11/13-2012/12/31

38. 超温R08-22、R1401甲烷化炉结构完整性评定, 2012/09/11-2012/12/31

39. E2001A水煤气废热锅炉管子管板连接处失效分析, 2012/06/20-2013/06/19

40. 氨泵用螺柱失效分析, 2012/05/08-2012/12/31

41. 工业纯锆挂样失效分析, 2012/04/06-2012/12/31

42. 20钢管金相组织及力学性能实验研究, 2011/04/08-2011/12/31

43. 矿井安全救生舱的应力和温度计算书分析及安全评定, 2011/03/18-2011/12/31

44. 关于联合开展材料性能微创测试技术研究, 2011/01/04-2011/12/31

45. 螺栓应力松弛分析与预防, 2010/08/02-2010/12/31

46. 材料分析, 2010/04/19-2010/12/31

47. 气化炉材料性能分析, 2010/06/24-2010/12/31

48. 螺旋板换热器失效分析, 2010/04/02-2010/12/31

49. 二厂3#6u50压缩机土入高压管丝头开裂分析研究, 2010/03/25-2010/12/31

50. 煤气发生炉开裂分析, 2010/03/15-2010/12/31

51. 高压超高压连续固体物料萃取和灭菌装置, 2009/10/21-2009/10/31

52. 一厂二期1800合成双甲高压管道材料性能和裂纹成因分析, 2009/12/09-2009/12/31

53. 热电厂75T锅炉20g热喷涂炉管泄漏原因分析, 2009/12/09-2009/12/31

54. 尿素塔检漏技术合作, 2008/12/04-2008/12/31

55. 阀盖事故分析, 2008/07/29-2008/12/31

56. 联箱管爆炸事故分析, 2008/07/29-2008/12/31

57. 20钢管性能恢复和最佳制造工艺条件试验研究, 2008/03/14-2008/12/31

58. 甲醛反应器寿命评估, 2008/01/16-2008/12/31

59. 氨分离器出口管爆炸原因分析, 2007/11/30-2007/12/31

60. 鲁西化工第三化肥厂尿素合成塔爆炸事故原因分析, 2005/03/29-2005/06/29

61. 中草药超临界萃取, 2005/02/05-2008/02/05

62. 柔性注液锚杆, 2004/12/20-2006/12/30

63. 农产品深加工及工业化设备研制, 2002/10/01-2006/12/01

64. 氟树脂高温耐蚀涂层配方性能与评价研究, 2002/01/01-2002/12/01

65. 设备检测, 2009/12/22-2009/12/31

66. 超临界流体连续萃取装置专利实施许可, 2009/10/08-2009/12/31

67. 20钢高压管道性能恢复研究, 2007/04/10-2007/04/10

68. 层板包扎高压容器剩余寿命试验评价技术, 2006/12/10-2008/12/30

69. 往复式压缩机活塞杆剩余寿命估算, 2010/10/09-2012/12/31

70. 立管性能测试, 2010/04/27-2010/12/31

71. 超临界流体连续萃取装置(山东省) , 2013/12/01-2014/12/31

Copyright All Rights Reserved Shandong University Address: No. 27 Shanda South Road, Jinan City, Shandong Province, China: 250100
Information desk: (86) - 0531-88395114
On Duty Telephone: (86) - 0531-88364731 Construction and Maintenance: Information Work Office of Shandong University